Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra DS16 - PA1010 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra DS16:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid Terra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Medium-viscosity polyamide 1010

VESTAMID® Terra DS16 NC is a medium-viscosity PA 1010 basic polymer. VESTAMID® Terra DS16 is semi-crystalline, which is the reason for its high mechanical resistance and chemical stability. It absorbs only little water. As a result its mechanical properties vary little when exposed to changing environmental humidity, and the material features a high dimensional stability.
 
VESTAMID® Terra DS16 can be used to manufacture films with good transparency.

The high melting point of VESTAMID Terra DS16 compounds results in a high heat deflection temperature that can be advantageous for some applications.
 
VESTAMID® Terra DS16 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and the standard polyamides PA 6 and PA 66, which have a shorter chain length.

VESTAMID® Terra DS16 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
VESTAMID® Terra is a group of new poly­amides, the monomers for which are based entirely or partly on renewable raw materials.

VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-dodecanedioic acid (sebacic acid-S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, bio-based and renewable resources up to 100%.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM

Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
성형 수축률, 평행 1.4 / * % ISO 294-4, 2577
성형 수축률, 수직 1.5 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 1700 / 1250 MPa ISO 527
항복강도 54 / 48 MPa ISO 527
항복변형률 5 / 22 % ISO 527
파단시 평균신율 >50 / >50 % ISO 527
챠피 충격 강도 , +23°C N / N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C N / N kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 7 / 7 kJ/m² ISO 179/1eA
Type of failure C / C - -
챠피 노치드 충격 강도, -30°C 7 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 200 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 37 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 55 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 136 / * °C ISO 75-1/-2
비카트 연화 온도, B 171 / * °C ISO 306
선형 열팽창 계수, 평행 115 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 135 / * E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB / * class IEC 60695-11-10
테스트 두께 1.6 / * mm -
전기적 특성건조/응축단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.6 / - - IEC 62631-2-1
상대 유전뮬, 1MHz 3.1 / - - IEC 62631-2-1
부피 저항 >1E13 / 8.3E11 Ohm*m IEC 62631-3-1
전기 압력 37 / - kV/mm IEC 60243-1
기타 특성건조/응축단위시험규격
물에서의 흡수성 1.8 / * % ISO 62와 유사
조건에서의 흡습성 1.4 / * % ISO 62와 유사
밀도 1040 / - kg/m³ ISO 1183
특징
생산 공정
사출 성형, 필름 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이), 과립
특별 특성
열안정성, 투명도
내화학성에
General Chemical Resistance
Certifications
Contains renewable resources
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.